Thermo-mechanical properties of C/SiC composite structure ...
The composite specimen is shown in Fig. 1 and was composed of a rectangular plate that was 210 mm long, 160 mm wide, and 8 mm thick. The preparation process of C/SiC composite specimens is described as follows. The unidirectional fiber cloths made of T700 carbon fiber of 12k yarn were stacked alternately with an orthogonal direction (0°/90°); a reticulated fabricated cloth is layered into ...